We are installing SS 310 skin thermocouple with heat shield in our DCU. The tube material is A335 P9. Our integrity department insist we perform buttering and PWHT for the installation. My questions:
1. Anybody have experience in such installation of skin TI where you have buttering and PWHT due to the dissimilar material weld? Does the TI's perform properly?
2. Is it a practice to have buttering and pwht for the installation? Buttering is due to dissimilar metal welding and PWHT is the requirement due to P9 material.